low thermal conductivity 1600C ceramic fiber modules for heat treatment furnace
low thermal conductivity 1600C ceramic fiber modules for heat treatment furnace
low thermal conductivity 1600C ceramic fiber modules for heat treatment furnace
low thermal conductivity 1600C ceramic fiber modules for heat treatment furnace

Review

Description

1600°C Classification Temperature Polycrystalline Ceramic Fiber Modules (Maximum Continuous Operating Temperature 1450°C)

Classification Temperature: 1600°C (Short-term tolerance)
Continuous Operating Temperature: ≤ 1450°C (Long-term stable use)
Core Advantages: Ultra-high temperature resistance, low thermal conductivity, thermal shock resistance, lightweight and modular design 

Main Application Areas
1. High-temperature Industrial Furnace Linings
Steel Metallurgy
- Permanent layer insulation for ladles and tundishes
- Inner lining of heat treatment furnaces (annealing, quenching)
Glass Industry
- Back insulation for hot spots in glass melting furnaces
- Upper insulation modules for tin baths
Ceramics/Refractory Materials
- High-temperature section lining for tunnel kilns and shuttle kilns 
2. Petrochemical and Energy Equipment
- Insulation layer for the radiant section of petrochemical cracking furnaces
- Thermal insulation for hot air ducts in power plant boilers
- Linings for polysilicon reduction furnaces 
 3. Laboratory and Specialized Equipment
- All-fiber lining for laboratory high-temperature furnaces (muffle furnaces, tube furnaces)
- Insulation barriers for single-crystal silicon growth furnaces
- Aerospace material testing equipment 
4. Other Harsh Environments
- Insulation for molten aluminum flow channels/casting systems
- Protection for the secondary combustion chamber of hazardous waste incinerators 

Comparison with traditional materials

Characteristics

Traditional Refractory Bricks

1600C Ceramic Fiber Module

highest continuous operating temperature

1350C

1450C

Thermal shock resistance

Poor(easy to cracking)

Well(no peeling occurs during rapid cooling and heating)

installation

Nee to be constructed(3-5 days)

Modular assembly




Chemical Composition

Al2O3

72%

Al2O3+SiO2

99%

Thermal Conductivity

1250℃

0.337w/m.k

1350℃

0.387w/m.k

Linear Shrinkage

1450℃×24hr

 

1.5%

Classification Temperature

1600℃

Bulk Density

180±10kg/m3